Wills Crackle Base

Wills Crackle Base

Firing temperature : cone 5-6 | Surface texture : glossy | Color : blue green | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

*Additives for Wills Saturated.

This is a very runny glaze. Use very thinly to inlay into carved lines or apply using a glaze trailer. The Wills Saturated variation is a dark teal green when thick and orange-brown when extremely thin. Extra silica was added in order to decrease the runniness and make a stronger glass.

This recipe was shared by Shana Salaff in the March/April 2019 issue of Pottery Making Illustrated.