Firing temperature : Cone 6 | Surface texture : matte | Color : white | Atmosphere: Oxidation/Neutral Reduction

Originally published in the May 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

Mix in red iron oxide by eye for a darker color. Mix to specific gravity of 1.2–1.25 for spray application.

For a straw color, add 1-5% Rutile.