Firing temperature : Cone 6 | Surface texture : matte | Color : white | Atmosphere: Oxidation/Neutral

Published in "Fumiya Mukoyama's Zogan Yusai" by Naomi Tsukamoto, in the Jan/Feb 2010 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

Fired to 2264°F (1240°C) in a gas kiln—in an oxidizing atmosphere.