White Liner Glaze (Blue)
Firing temperature : cone 5 | Surface texture : glossy to satin | Color : light blue | Atmosphere: Oxidation/NeutralPublished in "In the Potter's Kitchen: Easy and Elegant Butter Dish," in the July/August 2018 issue of Pottery Making Illustrated.
The image shown here has multiple glazes on it.
Ingredients
- 3.30
- 9.91
- 11.79
- 15.09
- 22.64
- 4.72
- 13.21
- 19.34
- 1.89
- Lost your password? Create New Password
- No password? Sign up
Add:
Instructions
This recipe can be poured or brushed on with great results and can be used as a base to make different colored glazes.