Firing temperature : Cone 6 | Surface texture : matte | Color : cream | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

This glaze will give a cream-colored matte surface when applied thinly and break into rivulets of gloss blue-white where thicker. Use with caution: it runs!

This recipe was shared by Marc Egan in the March/April 2020 issue of Pottery Making Illustrated.