V.C. Matte

Firing temperature : Cone 6 | Surface texture : matte | Color : clear | Atmosphere: Oxidation/Neutral

The piece in the image shown here was glazed with Ashleigh's Rivulet and Frasca Ash (green), and Hannah Fake Ash over V.C. Matte glaze.

Originally published in the Sept/Oct 2017 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

This glaze is a matte glaze and does not run if applied by itself. The glaze shown in the image above is a combination of V.C. Matte (applied first), Ashleigh's Rivulet, Frasca Ash (green), and Hannah Fake Ash.

Warning: Ash glazes and the glaze combinations listed and shown above can and do run during the firing. Plan accordingly to protect your kiln and kiln shelves. Ian Hall-Hough side fires all of his pieces with runny glazes on seashells and wadding, which are then placed and fired on a drip tray (a waster slab that has been bisque fired and is used during the glaze firing to catch the glaze that runs off the pots). After the firing, Ian uses a rubbing stone and/or a Dremel to clean up any sharp edges shells to remove and leftover white powder (calcium oxide) that is left after the firing.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend