Firing temperature : Cone 6 | Surface texture : satin to glossy | Color : clear | Atmosphere: Oxidation/Neutral

This glaze comes from Val Cushing (when you see V.C. in any recipe title, it probably refers to Cushing). The glaze breaks nicely over textured areas. I use it as a liner glaze on my vessel forms.

Originally published in the October 2017 issue of Ceramics Monthly.