Firing temperature : cone 6-7 | Surface texture : matte | Color : turquoise | Atmosphere: Oxidation

This recipe was shared by Susan Beiner in the December 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

This glaze is applied in a medium-thick application and fired to a hot cone 6 in a gas kiln. This glaze is not food safe.

I use several heavily fluxed base glazes combined with a variety o Mason stains, rare earth oxides, and encapsulated pigments to create palettes of color to glaze in a more painterly manner. Multiple glazes overlap, which influences how the glazes move across the forms. I am continually testing glazes and looking for interesting overlaps. Glaze application is done with a spray gun and bulb syringe. I draw glaze using a bulb syringe to further increase the mixing and melting of the glazes.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend