Ceramic Recipes logo

Tony Hansen’s G2934 Base Glaze

Tony Hansen's G2934 Base Glaze

Firing temperature : Cone 6 | Surface texture : matte | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This recipe was shared by Dan Ingersoll in the May/June 2020 issue of Pottery Making Illustrated.