Tony Hansen 20×5

Tony Hansen 20x5

Firing temperature : Cone 6 | Surface texture : matte to satin | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

A versatile clear base that can be colored with various oxides. The flux can also be substituted with others for different surface and color responses. I substituted Forshammer feldspar (a Swedish feldspar) for the Custer feldspar and Frit JM 169 for the Ferro frit 3134.

This recipe was shared by Alisa Liskin Clausen in the May 2019 issue of Ceramics Monthly.

 