Tomato Red Base (Tile 6)
Firing temperature : Cone 6 | Surface texture : glossy to satin | Color : red | Atmosphere: OxidationIngredients
- 5.0
- 6.0
- 18.6
- 13.0
- 10.1
F-4 Feldspar (sub. Minspar 200)
32.7- 3.4
Instructions
This recipe was shared by Ryan Coppage in the November 2019 issue of Ceramics Monthly.