Firing temperature : Cone 6 | Surface texture : textured | Color : medium blue | Atmosphere: Reduction

Published in "Glaze Forward" by Diana Pancioli, in the Jun 2006 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This is Marcia Selsor’s Waxy White base with a number of colorants added. This variation was derived from a 50/50 color blend with rutile incorporated in the base for texture. Goes glossy on interiors and breaks beautifully over textures.