Stony Earth Glaze

Firing temperature : cone 6-8 | Surface texture : satin | Color : brown | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Specific gravity: 1.43. Stony Earth Glaze has an earthy brown and green color, with simple ingredients. No extra red iron oxide was added for the base test. Additions of red iron oxide from 2% and up resulted in an overall dark brown gloss. My tests with red iron oxide added in increments from 1–5% made the glaze darker, and finally a dull brown gloss with 5%.

Forshammer feldspar is a combined soda and potash feldspar. In the US, test with Custer feldspar, Minspar 200 feldspar, and a 50/50 mix of Custer feldspar and Minspar 200 feldspar.

Original recipe shared by Patrick Fleming in the April 1980 issue of Ceramics Monthly.

This recipe was shared by Alisa Clausen in the February 2020 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend