Smooth and Stony Glaze with Red Iron Oxide

Firing temperature : Cone 6 | Surface texture : satin | Color : brown | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Specific gravity: 1.43. The surface of this glaze lives up to its name as a smooth and stony matte. The color response is not as vivid as it would perhaps be without the added magnesium carbonate. With cobalt carbonate, it is in the lilac range and with copper carbonate, it is a pale green. This glaze is not food safe. For color variations, omit the zinc oxide.

Original recipe shared by Rick Malmgren in the February 1980 issue of Ceramics Monthly.

This recipe was shared by Alisa Clausen in the February 2020 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend