Slate Blue K-15

Firing temperature : Cone 6 | Surface texture : satin matte | Color : blue | Atmosphere: Oxidation/Neutral Reduction

Published in "Mid-Range Mattes" by Holly Goring, in the January 2017 issue of Ceramics Monthly.

This is a very stable and dense satin matte glaze.


Click Image to Enlarge

Instructions

This base works well with other colorants. It is brightest on a porcelain or white stoneware clay body.