SJC Turquoise/Red Glaze

SJC Turquoise/Red Glaze

Firing temperature : Cone 6 | Surface texture : satin matte | Color : turquoise green | Atmosphere: Oxidation/Neutral Reduction

Published in "My Way With Clay" by Rick Malmgren, in the Oct 2000 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This image shows the SJC Turquoise sprayed over the Annette Florida Tan Glaze.

A glassy green in oxidation; in reduction a bright red.  Good when used to overlap other glazes.  When sprayed over Annette's Florida Tan, it gives a highly speckled look, particularly where thin.  The 2 base glazes can be colored with different coloring oxide and still give the same speckled look when they overlap.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend