Silky Matte G1214Z

Firing temperature : Cone 6 | Surface texture : matte | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This clear glaze is used on the interior of my functional pieces. It blends well with the polished porcelain and isn't distracting to my carved designs. Recipe originally from Digitalfire (https://digitalfire.com).

This recipe was shared by Joann Axford in the September/October 2019 issue of Pottery Making Illustrated.