Shelly’s Blue
Firing temperature : Cone 6 | Surface texture : glossy | Color : turquoise blue | Atmosphere: Oxidation/NeutralPublished in "Glazing Patterns" by Frank James Fisher, in the Nov/Dec 2006 issue of Pottery Making Illustrated.
Ingredients
- 4
- Lost your password? Create New Password
- No password? Sign up
Enter Your Log In Credentials

Send this to a friend
Comment
Comment
Love this glaze ! However, getting a lot of pin holing with a 2 and 3 layer dip. Any recommendations
Comment
Comment
What is the atmosphere? OX or RED?
Comment
Comment
Thanks to Lanse Stover for catching a typo in this recipe! It has 1.5% Copper Carb., not 91.5%
Good eye, Lanse.
Sherman Hall—admin