Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Beautiful high-gloss glaze that works well with the addition of Mason stains. This recipe is from Peter Pincus.

This recipe was shared by Kelly Justice in the March/April 2019 issue of Pottery Making Illustrated.