Firing temperature : cone 6-8 | Surface texture : glossy to satin | Color : white | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This is a cone-6 glaze that I fire cone 8 (using a witness cone) and hold for 10 minutes at the end of the firing. This glaze is fairly stable, but runs a little when fired hot. It breaks over texture beautifully. Add Epsom salts to the wet mix to keep the particles suspended. Apply to the thickness of a dime.

This recipe was shared by Jen Allen in the March 2020 issue of Ceramics Monthly.