Selsor Red + 4% Rutile

Firing temperature : Cone 6 | Surface texture : matte | Color : medium tan | Atmosphere: Reduction

Published in "Opaque Glazes" by John Britt, in the Oct 2014 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Shown on Frost porcelain.