Firing temperature : cone 6-8 | Surface texture : matte | Color : turquoise green | Atmosphere: Oxidation/Neutral

Published in "Cool Colors" by Linda Bloomfield, in the Feb 2012 issue of Ceramics Monthly.

 


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Calcium borate frit is an English frit similar in composition to colemanite with some added silica. American frits such as Ferro 3124, 3134, or 3195 can be substituted but they contain less boron and more silica. 'Borax frit' contains sodium, calcium, and boron similar to Gerstley borate and can be substituted with Ferro 3124 or 3134.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend