SDSU Texture/Crawl Glaze
Firing temperature : Cone 6 | Surface texture : glossy | Color : dark brown | Atmosphere: Oxidation/Neutral ReductionPublished in "My Way With Clay" by Rick Malmgren, in the Oct 2000 issue of Ceramics Monthly.
Ingredients
- 25
Instructions
SDSU was used on the ridges of this piece over the dipped Temmoku glaze.
Richard Burkett posted this glaze on clayart several years ago. It is very sensitive to thickness. Use by itself or over a contrasting glaze. Colorants can be added.