Reynolds Green Metal Patina

Firing temperature : Cone 6 | Surface texture : satin | Color : black | Atmosphere:

Click Image to Enlarge

Instructions

Apply by spraying, then remove excess glaze with a dry sponge to reveal the layers beneath.

This recipe was shared by Alan Johnson in the January/February 2021 issue of Pottery Making Illustrated.