Reynold’s Gold Metallic Glaze
Firing temperature : Cone 6 | Surface texture : matte | Color : gold | Atmosphere: Oxidation/Neutral ReductionPublished in "My Way With Clay" by Rick Malmgren, in the Oct 2000 issue of Ceramics Monthly.
Ingredients
- 4
- 2.5
- 36.5
- 49
Instructions
This image shows the Gold Metallic over Temmoku Glaze.
Works well in oxidation or reduction; however the color is more variegated in reduction. Manganese is toxic, and should be handled with extreme care. Never use this recipe on functional ware.