Raspberry Base Glaze

Raspberry Base Glaze

Firing temperature : cone 4-6 | Surface texture : glossy | Color : medium red | Atmosphere: Oxidation/Neutral

Published in "Tile Illustration: From Painter to Potter to Painter Again," by Paul Lewing, in the December 1989 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This is a chrome-tin pink glaze, which relies on a very specific ratio of tin and chrome.