Pinnell Celadon Revised

Pinnell Celadon Revised

Firing temperature : Cone 6 | Surface texture : matte | Color : medium green | Atmosphere: Reduction

Published in "Celadons at Six" by John Britt, in the Sep 2011 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

Use the same firing cycle as for cone 10 gas reduction, but simply stop it at cone 6/7.

You can substitute 1.5% strontium carbonate for the barium carbonate if you prefer.

Note: Synthetic red iron oxide is 96-99% pure red iron, made by calcining black iron oxide in oxidation. It is then milled to 325 mesh, which makes it ideal for celadons, because it will enter the melt more quickly and thoroughly. For more, see "All About Iron, page 14, March 2011 CM.

 

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend