Patti’s Crystal Clear

Patti's Crystal Clear

Firing temperature : cone 5–7 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

*Add colorant for Celadon.

This is a transparent glaze with a light blue tint. Apply a thin layer to avoid crazing. This is an excellent glaze base for adding colorants to create a palette of colors.

This recipe was shared by Ashley Kim in the March/April 2019 issue of Pottery Making Illustrated.