Firing temperature : cone 5-6 | Surface texture : glossy | Color : gold | Atmosphere: Oxidation/Neutral

This recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

This glaze isn’t stable (it’s very fluid), but when used in accent areas it forms nice pools and drips. Crackle glaze isn’t suitable for food surfaces.