Ceramic Recipes logo

Pablo’s Honey Gold

Firing temperature : Cone 6 | Surface texture : matte | Color : medium brown | Atmosphere: Oxidation/Neutral

Published in "Ohio Slip: Au Natural" by Paul Andrew Wandless, in the Jan/Feb 2009 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Single dip and fire. All recipes were screened with 60 mesh sieve and electric fired to 2291°F (cone 6).