Firing temperature : cone 6-8 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

P-Base is my liner glaze. I always sieve the glaze, mix it thoroughly, and apply it thin (about the consistency of 1% milk). I fire to cone 8 in oxidation; however, this glaze can be fired from cone 6–8.

This glaze was shared by Doug Peltzman in the December 2019 issue of Ceramics Monthly.