Opaque Matte #5
Firing temperature : Cone 6 | Surface texture : matte | Color : blue | Atmosphere: OxidationIngredients
- 19
- 9
- 52
- 15
- 5
- 10
- 10
Add:
Instructions
I program a 15-minute hold and slow cool at the end of the firing in an electric kiln. This gives a very soft matte finish with little sheen. Otherwise it is a bit waxy with a low sheen. I used Mason stain #6315 Zirconium Vanadium Blue as the colorant in the process images.
This recipe was shared by Alan Johnson in the January/February 2021 issue of Pottery Making Illustrated.