Odyssey Clear

Odyssey Clear

Firing temperature : cone 4-6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

A clear glaze designed to fire at cone 5 or 6. I fire it to cone 4 on Highwater Clay’s Earthen Red clay body and it works wonderfully. The fired results are best when the specific gravity is 1.4. If applied too thick, it can result in crawling or create a foggy look on top of underglaze.

This recipe was shared by Sara Ballek in the November/December 2020 issue of Pottery Making Illustrated.