Nucular Green
Firing temperature : Cone 6 | Surface texture : satin to glossy | Color : green | Atmosphere: Oxidation/NeutralOriginally published in the November 2017 issue of Ceramics Monthly.
Ingredients
- 14.2
- 11.7
- 50.6
- 5.0
Instructions
0.05% CMC gum can be added to this glaze to help prevent it from settling. This glaze has some opacity/ satin character.