Nate’s Red Stoneware

Nate's Red Stoneware

Firing temperature : cone 7 | Color : brown | Atmosphere: Reduction

Click Image to Enlarge

Instructions

Stancills Red Clay is a clay I source from a local mine. This is a great throwing body that fires dark brown in reduction.

This recipe was shared by Nathan Willever in the May 2019 issue of Ceramics Monthly.