Firing temperature : cone 5-6 | Surface texture : glossy to satin | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This base takes stains really well. I use up to 9% stain for fully saturated color swatches and smaller sections of glaze that I paint on, and 1–3% stain in my liner glaze palette choices. This recipe was shared by Richard Burkett in San Diego, California.

This recipe was shared by Deb Schwartzkopf in the March 2019 issue of Ceramics Monthly.