N502 Transparent and Glossy with 5% Titanium Dioxide
Firing temperature : cone 5 | Surface texture : glossy | Color : blue | Atmosphere: OxidationIngredients
- 30
F-4 Feldspar (sub G200 Feldspar)
46- 13
- 11
Add:
Instructions
Add titanium dioxide to make this clear glaze more opaque.
This recipe was shared by Yoko Sekino-Bové in the April 2021 issue of Ceramics Monthly.