Ceramic Recipes logo

N502 Transparent and Glossy with 10% Tin Oxide

N502 Transparent and Glossy with 10% Tin Oxide

Firing temperature : cone 5 | Surface texture : glossy | Color : blue | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Adding 10% tin oxide makes this clear glass opaque.

This recipe was shared by Yoko Sekino-Bové in the April 2021 issue of Ceramics Monthly.