N502 Transparent , Glossy + CuCo3 + TiO2

N502 Transparent , Glossy + CuCo3 + TiO2

Firing temperature : cone 5 | Surface texture : glossy | Color : dark green | Atmosphere: Oxidation/Neutral

Published in "Expanding Your Palette in Mid-Range Firing" by Yoko Sekino-Bové, in the Jan 2011 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments
  • Mary Alice C.

    N502 is very reliable and not finicky at all. I have fired using several firing schedules with success each time. It takes color well also.