N502 Transparent and Glossy + CuCo3 and SnO2

N502 Transparent and Glossy + CuCo3 and SnO2

Firing temperature : cone 5 | Surface texture : glossy | Color : light blue | Atmosphere: Oxidation/Neutral

Published in "Expanding Your Palette in Mid-Range Firing" by Yoko Sekino-Bové, in the Jan 2011 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients