Meyers White

Meyers White

Firing temperature : cone 04-8 | Atmosphere: Oxidation/Neutral

Published in "Pour It On! Recipes" by Carly Van Anglen and David Ferro, Alina Hayes, and Justin Donofrio in the September 2017 issue of Ceramics Monthly


Click Image to Enlarge

Instructions

Add Epsom salts for suspension. Rub out large pinholes before firing. Overly thick application can lead to pinholes where glaze pools. Higher temperature will give you more movement and color trails. Works with all forms of glaze applications.

For colors, add Mason stains (MS).

For Blue, add: 1.5% MS Robins Egg 6376, 0.25% MS Sky Blue 6363, and 0.25% MS Slate 6531.

For Green, add: 1% MS Avocado 6280 and 0.5% MS Slate 6531.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend