Marilee’s Lava Glaze

Marilee’s Lava Glaze

Firing temperature : Cone 6 | Surface texture : textured | Color : black | Atmosphere: Oxidation/Neutral Reduction

Published in "My Way With Clay" by Rick Malmgren, in the Oct 2000 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

A very rough glaze; not intended for food surfaces.  Fine silicon carbide seems to work best. For a gray to black variation, add 70% Mason stain 6600.