Ceramic Recipes logo

Manganese Mix

Manganese Mix

Firing temperature : cone 7 | Surface texture : satin | Color : brown | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Not food safe without a glaze applied over top. My terra cotta clay can be fired to a maximum temperature of 2282°F (1250°C), approximately cone 7. Test with your local clay to find the right temperature.

This recipe was shared by Mizuyo Yamashita in the June/July/August 2019 issue of Ceramics Monthly.