M & M Altered – CoO
Firing temperature : cone 5-6 | Surface texture : matte | Color : cobalt blue | Atmosphere: Oxidation/NeutralPublished in "Silicon Carbide: The Stuff of Stars" by Mark Chatterley, in the Mar 2011 issue of Ceramics Monthly.
Ingredients
Gerstley Borate (sub Gillespie Borate)
18- 16
- 40