Ingredients

Instructions

Paint this wash lightly over the glaze to encourage running. (Painted over EM Satin on selected areas of color and lines.) Recipe shared by Chandra DeBuse.

Commercial products used:

Amaco HF9 Zinc-Free Clear (painted over selected areas to keep glossy and crisp line)

Amaco Satin Matte Glazes: SM63 Yellow, SM27 Teal, SM42 Mint

Amaco Underglazes: V361 Jet Black for inlay, V375 Maroon

Duncan Premium Gold Luster

This recipe was shared by Stephanie Wilhelm in the November 2019 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend