Firing temperature : Cone 6 | Surface texture : matte | Color : black | Atmosphere: Oxidation/Neutral

Published in "Glazing Patterns" by Frank James Fisher, in the Nov/Dec 2006 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients