John’s 10x Series #12

Firing temperature : Cone 6 | Surface texture : matte | Color : medium brown | Atmosphere: Oxidation/Neutral

This recipe was used to test the opacifiers Zircopax, Tin Oxide, and Titanium Dioxide, from 2–10%. The image shown here displays the range of results.

Published in "Opacifiers" by Dave Finkelnburg, in the Oct 2014 issue of Ceramics Monthly.