Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This is a runny clear glaze. I brush it on thickly to get bigger drips.

This recipe was shared by Jill Birschbach in the September 2020 issue of Ceramics Monthly.