Firing temperature : Cone 6 | Surface texture : glossy | Color : amber | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

This is the base glaze I use on my cup forms. I add colorants to achieve the yellow and blue-gray tones, and use a thick application to achieve the dripping effects. The glaze comes from Mastering Cone 6 Glazes by John Hesselberth and Ron Roy (page 89).

This recipe was shared by Branan Mercer in the September 2019 issue of Ceramics Monthly.

 