Firing temperature : cone 7 | Surface texture : glossy | Color : clear | Atmosphere: Reduction

Click Image to Enlarge

Instructions

A clear glaze that will work well in oxidation and reduction. I use it very thin at a specific gravity of 1.32. If applied too thinly, the glaze will be a rough white. Applied too thick, it will be gray.

This recipe was shared by Nathan Willever in the May/June 2019 issue of Pottery Making Illustrated.